I believe so. The problem I was having was bubbles would come back after an hour or so. But I changed the lamination process from 2 mins to 5 seconds, and I also was not laying the oca on the glass correctly bc I was not using the machine that aids you in laying the oca on the glass correclty. After I laid oca on glass good and changed lamination settings then I got no bubble return.

also another thing to note is after lamination process do not press on glass to try and squeeze out the air bubbles. Let the autoclave do that. I use to press on the glass after lamination to try and squeeze the big bubbles out so the autoclave wouldnt have to remove big bubbles, but I had better sucess rate with no hard pressing
  Reply With Quote
The Following 2 Users Say Thank You to cellularman89 For This Useful Post:
 
Page generated in 0.08580 seconds with 7 queries