When i posted i was using a oca that i donīt even know itīs brand. Now iīm using mitsubish. Since i started using mitsubish, i am having the same problem you had. No bubbles right after autoclave. 1 or 2 bubble come back couple hours later.

I am laminating manually. Like this video on youtube (i canīt post links): How do Chinese laminate the OCA adhesive on the glass of your cell phone

then put the glass (manually) on the lcd and then autoclave. The only machine i use is autoclave

About the autoclave. You said you use 4 or 5 mpa pressure. Itīs a lot of pressure. I am using 60 or 70 PSI, thats equal to 0,4 or 0,5 mpa. To avoid miss understanding, can you send a picture of you manometer when the autoclave is on the right pressure?